Passivating Pickling Paste is highly concentrate paste which is used to clean weld seams and surrounding areas and is applied with brush. This is very effective product to acts as Degreasing, cleaning, pickling and passivation.
Feature | Description |
---|---|
Powerful Weld Scale Remover | Effectively removes welding burns, discoloration, and oxides from stainless steel surfaces. |
Thixotropic Gel Form | Thick paste adheres easily to vertical and overhead surfaces without dripping or running. |
Restores Corrosion Resistance | Removes surface impurities and oxide layers to restore the natural passive film of stainless steel. |
Easy to Apply & Rinse | Can be applied with brush or spatula; rinses off easily with water after the reaction time. |
Ideal for SS316, SS304, etc. | Suitable for all common grades of stainless steel, ensuring universal usability in industry. |
Surface Brightening Effect | Leaves a uniform, clean, and bright finish after treatment—ideal for aesthetic and hygienic applications. |
Reduces Rework & Surface Grinding | Eliminates the need for abrasive cleaning or polishing in many cases. |
Safe Packaging | Available in tamper-proof, sealed containers for safe transport and handling. |
Custom Reaction Time | Fast-acting formula typically requires 10–30 minutes based on the extent of oxidation or scale. |
Share

RX Jelly Pickling Paste supplier in UAE
Application :
It is used to remove heavy scales, discolouration, annealing colours, rust particles near weld and welding affected area by heat without grinding or wire brushing or buffing.
Coverage : Approx. 100 meters of running weld seam / kg of Passivating Pickling Paste.
Dose : -
For Stain :
1.Passivating Pickling Paste is applied on weld seam & surrounding areas with a nylon bristled plastic brush. Application Temp. = between 5 – 40 deg. C
2. Keep Passivating Pickling Paste for 5 to 30 minutes (contact time) depending on contamination, temperature & grade of Stainless Steel.
3. Use pressurised water jet spray OR wipe the weld seam lightly with plastic brush & wash with water thoroughly.
For Satin / Dull Finish
1. First remove oil, dirt, buffing compounds etc, with Rxsol Degreaser. Add 50-75 gm/lit. in water (i.e. 1 kg Rxsol Degreaser in 15 to 20 lit. water) & stir to dissolve. Wipe S.S surface with cotton cloth or pressurized spray for 2-5 min. or soak for 10 min. Then, wash with water properly.
2. Passivating Pickling Paste is applied on weld seam & surrounding areas with a nylon bristled plastic brush or by Paste sprayer or circulated in pipeline with pump.
Application Temp. = Room temp.( i.e. between 25-35 C). If temperature is less than 25 C, then more time may be required and if temperature is more than 35 C, then uneven preocessing & drying of applied materials may result.Then, cool SS equipment by keeping it in shade or cover by temporary shade to protect sun light.
3.Keep Passivating Pickling Paste for 10-45 minutes depending on contamination & scale. (Passivating Pickling Paste generally kept for 10-30 min. and Pickling Spray generally kept 30-45 min. Depending on SS type and initial condition of SS parts)
4. Wipe the weld seam lightly with plastic brush or cloth & wash the Passivating Pickling Paste applied area with water thoroughly.
5.Spray or Dip in Passivate 1 or Passivate - 2 Solution & leave it for 15-25 minutes. Rinse with water thoroughly. ( Steps 1 & 5 can be avoided for Passivating Pickling Paste on weld seam application)
For passivating Mirror Bright SS Areas
THE BELOW STEPS WILL NOT AFFECT SHINE OF MIRROR BRIGHT POLISHED SS AREAS AND PROVIDE CONTAMINATION & STERILE PARTICLE FREE PASSIVATED SS SURFACE.
1) First apply Passivating Pickling Paste in weld seam & surrounding areas with a nylon bristled plastic brush. After 10 to 30 min. wipe with cloth or plastic brush & wash water thoroughly.
(Application of Passivating Pickling Paste ensures that black & red spots do not come on & near weld seams area as generally observed some days after bright buffing.)
2) Complete bright buffing / polishing procedure to make surface mirror bright & shiny.
DISCARD STEPS 1 & 2 ABOVE, IF SS SURFACE IS ALREADY BRIGHT BUFFED OR ELECTROPOLISHED.
3) Remove oil, dirt buffing compounds etc. with RXSOL Degreaser which is Metal Free Degreaser. Add 50-75 gm/lit. in water & stir to dissolve.
Wipe S.S. surface with cotton cloth or pressurised spray for 2-5 min. or soak small parts for 10 min. Wash with water prpoerly.
4) Spray or Dip in Passivate - 1 or Passivat -2 & leave it for 15-25 minutes. then rinse with water thoroughly.
NOTE: It is better to rinse SS surface with 10 gm/lit RXSOL DEGREASER solution as the last step and then rinse with water to ensure complete removal of previously applied Passivate Pickling paste or spray from the surface.
Properties :
Appearance: Liquid, viscous, colourless, soluble in water
pH : <1 at 1 % concentration
Boiling point : - not known
Vapour pressure : <0.01 kPa at 20 deg C
Vapour density : not known
Freezing point : <0 °C at 760 mm/Hg
Solubility in Water :Completely soluble in water
Advantage & Benifit
- Easy to apply.
- Due to paste easy to use on vertical surface.
- Simply washed with water.
- Easy to handle.
- Easly remove heavy scales, discolouration, annealing colours, rust particles near weld and welding affected area .
RX Jelly Pickling Paste manufacturer in UAE
View all-
Environmentally Friendly Corrosion Inhibitors f...
Environmentally Friendly Corrosion Inhibitors for Sustainable Cooling Water Treatment Keywords: eco friendly corrosion inhibitor GCC, green water treatment UAE, sustainable cooling tower chemicals Oman, biodegradable inhibitor Middle East Introduction With...
Environmentally Friendly Corrosion Inhibitors f...
Environmentally Friendly Corrosion Inhibitors for Sustainable Cooling Water Treatment Keywords: eco friendly corrosion inhibitor GCC, green water treatment UAE, sustainable cooling tower chemicals Oman, biodegradable inhibitor Middle East Introduction With...
-
How Corrosion Affects Energy Efficiency in Cool...
How Corrosion Affects Energy Efficiency in Cooling Towers – And How to Fix It Keywords: corrosion and energy loss, cooling tower efficiency GCC, rust inhibitor UAE, cooling water optimization Saudi...
How Corrosion Affects Energy Efficiency in Cool...
How Corrosion Affects Energy Efficiency in Cooling Towers – And How to Fix It Keywords: corrosion and energy loss, cooling tower efficiency GCC, rust inhibitor UAE, cooling water optimization Saudi...
-
Corrosion Inhibitors vs. Scaling Inhibitors – D...
Corrosion Inhibitors vs. Scaling Inhibitors – Do You Need Both in GCC Cooling Towers? Keywords: corrosion vs scaling inhibitors, scale and corrosion control GCC, cooling water chemicals UAE, inhibitor for...
Corrosion Inhibitors vs. Scaling Inhibitors – D...
Corrosion Inhibitors vs. Scaling Inhibitors – Do You Need Both in GCC Cooling Towers? Keywords: corrosion vs scaling inhibitors, scale and corrosion control GCC, cooling water chemicals UAE, inhibitor for...